Mainly increase toughness and strength of plastic scraping, regrinding and raw materials
Surface of product bright without flawing
Intimates comrade for plastic modification and increases amount of filling materials
Dosage: 2 to 4%, Be sure that 25kg plastic sample is used and mixed in blender for 5 to 8 minutes
Added in process of blending materials
Toughening agent is blended with plastic scraping, regrinding and raw materials for 5 to 8 minutes
When material has been uniformly blended, mixture material can be heated for extrusion and blow/injection molding
In order to test effect of toughening agent, please carry out it after that extrusion and injection/blow molding have be finished for 24 hours
That will make the effect more obvious
Please compare it with plastics of same material and try best to use plane product without hole [1] |